The effects of different solvents on the fabrication of organic photovoltaic cells by gravure printing are reported. Polymer bulk heterojunction solar cells were fabricated with ITO/PEDOT:PSS/P3HT: PCBM/Al layer structures using 4-9 wt% mixtures of poly(3-hexylthiophene) (P3HT) and [6,6]-phenyl-C61 butyric acid methyl ester (PCBM) in 1,2-dichlorobenzene to optimize solution viscosity for gravure printing. 7 wt% P3HT: PCBM showed optimal efficiency of 1.64% and resulted in an active layer 340 nm thick. Three solvents, 1,2-dichlorobenzene, chloroform, and chlorobenzene, were tested and a 1 : 1 ratio mixture of 1,2-dichlorobenzene and chloroform resulted in the best efficiency of 2.21%. This study demonstrates the importance of solvent effects in the gravure printing of organic photovoltaic devices.