Coke Formation on the Surface of α-Al2O3 in the Catalytic Pyrolysis of Naphtha
The catalytic pyrolysis of naphtha has been carried out in a quartz reactor loaded with 5 mm α-Al2O3 spheres, The yields of ethylene and propylene exhibit about 10% and 5% higher values compared to the thermal pyrolysis in the absence of α-Al2O3 spheres at the same reaction conditions. The coke formation on α-Al2O3 spheres increased continuously along with the axial length of the reactor as well as with reaction time. Results suggest that the concentration of the coke precursors in the gas phase may increase along with the axial length of the reactor. Coke filled up completely the internal pore of the sphere near the exit of the reactor after reaction for 4 hr. The coke film on the external surface of the sphere grew continuously thicker. The coke formation was influenced strongly by the physical properties of the α-Al2O3 spheres. Coke deposition was the least on the α-Al2O3 sphere with the lowest surface area and pore volume among the tested α-Al2O3 spheres.
[References]
  1. Adel'son SV, Zhagfarov FG, Rudyk EM, Smirnova GY, Zh. Fiz. Khim., 62, 2216, 1988
  2. Adel'son SV, Rudyk EM, Smirnova GY, Zhagfarov FG, Neftepererab. Neftekhim, 4, 21, 1985
  3. Albright LF, Crynes BL, Corcoran WH, "Pyrolysis-Theory and Industrial Practice," Academic Press, London, 1983
  4. Basu B, Kunzru D, Ind. Eng. Chem. Res., 31, 146, 1992
  5. Chan KYG, Inal F, Senkan S, Ind. Eng. Chem. Res., 37(3), 901, 1998
  6. Ghosh KK, Kunzru D, Ind. Eng. Chem. Res., 27, 559, 1988
  7. Golombok M, Kornegoor M, van den Brink P, Dierickx J, Grotenbreg R, Ind. Eng. Chem. Res., 39(2), 285, 2000
  8. Gueret C, Billaud F, Fixari B, Le Perchec P, Carbon, 33, 159, 1995
  9. Kumar P, Kunzru D, Can. J. Chem. Eng., 63, 598, 1985
  10. Kumar VA, Pant K, Kunzru D, Appl. Catal. A: Gen., 162(1), 193, 1997
  11. Lee KH, Ha BH, Korean J. Chem. Eng., 15(5), 533, 1998
  12. Lemonidou AA, Vasalos IA, Hirschberg EJ, Bertolacini RJ, Ind. Eng. Chem. Res., 28, 524, 1989
  13. Lemonidou AA, Koulouris AP, Varvarezos DK, Vasalos IA, Appl. Catal., 69, 105, 1991
  14. Mongkhonsi T, Prasertdham P, Saengpoo A, Pinitniyom N, Jaikaew B, Korean J. Chem. Eng., 15(5), 486, 1998
  15. Mukhopadhyay R, Kunzru D, Ind. Eng. Chem. Res., 32, 1914, 1993
  16. Reyniers MF, Froment GF, Ind. Eng. Chem. Res., 34(3), 773, 1995
  17. Speight JG, Korean J. Chem. Eng., 15(1), 1, 1998
  18. Srihiranpullop S, Praserthdam P, Mongkhonsi T, Korean J. Chem. Eng., 17(5), 548, 2000
  19. Xanthopoulou G, Appl. Catal. A: Gen., 182(2), 285, 1999
  20. Zou R, Lou Q, Mo S, Feng S, Ind. Eng. Chem. Res., 32, 843, 1993