articles This is an Open-Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/bync/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
Copyright © KIChE. All rights reserved.

All issues

TENSILE STRENGTH AND MORPHOLOGICAL INVESTIGATION OF SIC-COATED CARBON FIBERS

Korean Journal of Chemical Engineering, September 1995, 12(4), 416-420(5), 10.1007/BF02705804
downloadDownload PDF

Abstract

SiC-coated film onto carbon fibers as a barrier of oxidation resistance and reaction between carbon fibers and metals was investigated. The chemical vapor deposition of silicon carbide onto carbon fibers was performed at various temperatures ranging from 700 to 1000℃ using trilsopropylsilane vapor carried by hydrogen gas. The strength of the SiC-coated carbon fibers was decreased due to deterioration of fibers and chemical attack of hydrogen on the surface of carbon fibers during the coating process. The oxidation and the thermal resistance of the SiC-coated carbon fibers compared to the uncoated carbon fibers were improved at temperature range of 600-800℃ and 1000-1200℃, respectively. Morphological change by air oxidation at temperature range of 500-800℃ was also investigated for the SiC-coated and the uncoated carbon fibers, respectively. The SiC-coated film between carbon fiber and aluminum was sufficient as a barrier of reaction on carbon fiber reinforced aluminum at temperature of above 1000℃.

References

Aggour L, Fitzer E, Heym M, Ignatowittz E, Thin Solid Films, 40, 97 (1977) 
Baker SJ, Bonfield W, J. Mater. Sci., 13(6), 1329 (1978) 
Bunsell AR, "Fiber Reinforcements for Composite Materials," Composite Materials Series Vol. 2, Elsevier Science Publishers in Netherlands (1988)
Canmer DC, Am. Ceram. Soc. Bull., 68(2), 415 (1989)
Chin J, Gantzel PK, Hudson RG, Thin Solid Films, 40, 57 (1977) 
Dhami TL, Manocha LM, Bahl OP, Carbon, 29(1), 51 (1991) 
Guiden TD, J. Am. Ceram. Soc., 51(8), 424 (1968) 
Jones LE, Thrower PA, Carbon, 29(2), 251 (1991) 
Kobayashi K, Funabashi H, Uchiyama Y, Tanso, 151, 27 (1992)
Kohara S, Nuto N, J. Jpn. Inst. Metals, 44(4), 271 (1980)
Kohara S, Nuto N, Imanishi Y, J. Jpn. Inst. Metals, 43(7), 589 (1979)
Leonhardt G, Kieselstein E, Podlesak H, Than E, Hoffmann A, Mater. Sci. Eng., A135, 157 (1991) 
Masato K, J. Jpn. Inst. Metals, 42(2), 131 (1978)
Muench WV, Pfaffeneder I, Thin Solid Films, 31, 39 (1976) 
Noone NJ, Roberts JP, Nature, 212, 71 (1966)
Pitkethly MJ, Doble JB, Jacoues P, J. Mater. Sci. Lett., 12(18), 1439 (1993) 
Scholz M, Fub W, Kompa KL, Adv. Mater., 5(1), 38 (1993) 
Stumm T, Fitzer E, Wahi G, J. Phys. III France, 2(8), 1413 (1992) 
Warren R, Anderson CH, Carlsson M, J. Mater. Sci., 13(1), 178 (1978) 
Yamamoto O, Sasamoto T, Inagaki N, J. Ceram. Soc. Jpn., 102(2), 165 (1994)

The Korean Institute of Chemical Engineers. F5, 119, Anam-ro, Seongbuk-gu, 233 Spring Street Seoul 02856, South Korea.
Phone No. +82-2-458-3078FAX No. +82-507-804-0669E-mail : kiche@kiche.or.kr

Copyright (C) KICHE.all rights reserved.

- Korean Journal of Chemical Engineering 상단으로